(1) Zhang YN, et al.*, Strain engineering of particles and interfaces for long-life stable LiNi0.8Co0.1Mn0.1O2 cathodes, Energy Storage Materials, 2026,86: 104924. https://doi.org/10.1016/j.ensm.2026.104924 (2) Zhang YN, et al.*, Progress on the attenuation mechanism and modification of the cobalt-free spinel LiNi0.5Mn1.5O4 [J]. Advanced Science (2025) e08121.https://doi.org/10.1002/advs.202508121 (3) Zhang YN, et al.*, Dual functional coordination interactions enable fast polysulfide conversion and robust interphase for high-loading lithium-sulfur batteriey [J]. Materials Horizons (2025) 12: 1473-1485. https://doi.org/10.1039/d4mh01504e (4) Zhang YN, et al.*, Using high-entropy configuration strategy to design spinel lithium manganate cathodes with remarkable electrochemical performance [J]. Small (2025) 21: 2410999.https://onlinelibrary.wiley.com/doi/10.1002/smll.202410999 (5) Zhang YN, et al.*, Near-surface reconstruction in cobalt-free spinel positive electrodes for high-performance lithium-ion batteries [J]. Journal of Colloid and Interface Science(2026) 702: 138986https://doi.org/10.1016/j.jcis.2025.138986 |